Specs
► Meets ANSI / ESD STM 4.1 Standard
► Lead-Free. Recyclable. Meets European Union (EU) Restriction of Hazardous Substances Directive (RoHS) regulating the reuse of products used in electrical and electronic equipment.
| Properties | Units | Typical alues | Test Method |
|---|---|---|---|
| Material | - | Nitrile Butadiene Rubber / Carbon | - |
| Thickness | Inches | .08 | ASTM D-2103 |
| Thickness | Millimetres | 2 | ASTM D-2103 |
| Tensile Strength • Top Layer | kg / sq. cm | > 120 | ASTM D-412 |
| Tensile Strength • Bottom Layer | kg / sq. cm | > 160 | ASTM D-412 |
| Tear Strength • Top Layer | kg / sq. cm | > 90 | ASTM D-412 |
| Tear Strength • Bottom Layer | kg / sq. cm | > 100 | ASTM D-412 |
| Elongation • Top Layer | % | 350 | ASTM D-412 |
| Elongation • Bottom Layer | % | 250 | ASTM D-412 |
| Hardness • Top Layer | Shore A | 50 | ASTM D-2240 |
| Hardness • Bottom Layer | Shore A | 60 | ASTM D-2240 |
| Gravity • Top Layer | - | 1.3 | ASTM D-792 |
| Gravity • Bottom Layer | - | 1.4 | ASTM D-792 |
| ESD Surface Resistance • Top Layer | ohms / square | < 109 | ASTM D-257 |
| ESD Surface Resistance • Bottom Layer | ohms / square | < 105 | ASTM D-257 |
| Volume Resistivity • Top Layer | ohms / square | < 108 | ASTM D-257 |
| Volume Resistivity • Bottom Layer | ohms / square | < 104 | ASTM D-257 |
| Static Decay | seconds | < 0.01 | EIA-541 |
| Temperature Tolerance | Fahrenheit / Celsius | 187F / 86C | - |